2008 · 19 citations · 13 references
EngineeringElectrical EngineeringMaterials ScienceMicroelectronicsSemiconductor DevicesSemiconductor MaterialsComplementary Metal-oxide-semiconductor TechnologyDevice CharacterizationDevice ReliabilityOxide SemiconductorsSemiconductor Device MaterialsSemiconductor ReliabilityCmos ReliabilityGate Oxide DegradationGate Oxide ReliabilityGate OxidesLifetimesOxide ReliabilityReliability DegradationReliability Degradation Mechanisms
NBTI degradation and recovery have been investigated for 7 to 50nm oxides and compared to a thin 2.2nm nitrided oxide. A wide regime of stress fields 2.5MV/cm to 8MV/cm has been covered. NBTI effect for the nitrided oxide is larger than for non-nitrided oxides. The percentage of threshold shift DeltaVth which is "lost" during a long measurement delay - which is the quantity leading to curved DeltaVth vs stress-time curves and to errors in extrapolated lifetimes - is about equal for nitrided or thick non-nitrided oxides. The fraction of recovered DeltaVth is strongly dependent on stress time but only weakly dependent on stress field. Recovery in thick oxides leads to exactly the same problems as for non-nitrided oxides and clearly a fast measurement method is needed.
13
Electronic properties of two-dimensional systems
Tsuneya Ando, A. B. Fowler, Frank Stern · Reviews of Modern Physics · 1982 · 7.4K citations
Natural Sciences, Chemistry, Physics +16