IEEE International Reliability Physics Symposium proceedings · 2009 · 211 citations · 48 references
Natural SciencesMaterials SciencePhysicsCondensed Matter PhysicsElectronic MaterialsSemiconductor MaterialsAmorphous MaterialsAmorphous SolidsDefect ModelingDefects In Electronic MaterialsSemiconductor DefectsSemiconductor ReliabilityAmorphous OxidesAnnealingAnnealing ProcessesBias Temperature InstabilityDefects In Amorphous MaterialsNegative Bias Temperature InstabilityOxide Defect StatesOxygen Vacancy Formation
Based on the established properties of the most commonly observed defect in amorphous oxides, the E' center, we suggest a coupled two-stage model to explain the negative bias temperature instability. We show that a full model that includes the creation of E' centers from their neutral oxygen vacancy precursors and their ability to be repeatedly charged and discharged prior to total annealing is required to describe the first stage of degradation. In the second stage a positively charged E' center can trigger the depassivation of P <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">b</sub> centers at the Si/SiO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> interface or K <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">N</sub> centers in oxynitrides to create an unpassivated silicon dangling bond. We evaluate the new model to experimental data obtained from three vastly different technologies (thick SiO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> , SiON, and HK) and obtain very promising results.
48