2008 · 27 citations · 20 references
EngineeringElectrical EngineeringMaterials EngineeringElectronic MaterialsMetallurgySemiconductor DevicesAlloysDevice ReliabilityMetal-semiconductor ContactsMetalsSemiconductor ReliabilityCurrent CrowdingElectromigrationElectromigration AnalysisElectromigration ReliabilityMetallizationSoldered JointsSolderingSoldering Joints
The Cu pillar is a thick under bump metallurgy (UBM) structure developed based on the consideration of alleviating current crowding in a flip-chip solder joint in operation conditions. We present in this work electromigration reliability and morphologies of Cu pillar flip-chip solder joints formed by joining Ti/Cu/Ni UBM with largely elongated Cu at ~62 mum onto Cu substrate pad metallization through the Sn-3Ag-0.5Cu solder alloy. Three test conditions that controlled averaged current densities in solder joints and ambient temperatures were considered: 10 kA/cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sup> at 150degC,10 kA/cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sup> at 160degC, and 15 kA/cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sup> at 125degC.Electromigration reliability of this particular solder joint turns out to be much enhanced compared to a conventional solder joint with thin-film-stack UBM. Cross-sectional examinations of solder joints upon failure indicate that cracks formed in (Cu,Ni) <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">6</sub> Sn <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">5</sub> or Cu <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">6</sub> Sn <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">5</sub> intermetallic compounds (IMCs) near the cathode side of the solder joint. Moreover, the ~52 mum thick Sn-Ag-Cu solder after long-term current stressing has turned into a combination of ~80% Cu-Ni-Sn IMC and ~20% Sn-rich phases, which appeared in the form of large aggregates that in general distributed on the cathode side of the solder joint.
20
Ag3Sn plate formation in the solidification of near-ternary eutectic Sn-Ag-Cu
Sung K. Kang, Da‐Yuan Shih, NY. Donald et al. · JOM · 2003 · 164 citations