EngineeringElectrical EngineeringPhysicsCondensed Matter PhysicsSemiconductor DevicesSemiconductor MaterialsCarrier TransportDevice ModelingSemiconductor DefectsSemiconductor Device MaterialsSemiconductor PhysicsCarrier ConcentrationCarrier Mobility ModelingHall ConductivityHall EffectSilicon CarbideSilicon Carbide (Sic) MaterialsTemperature Dependence
Hall measurements on NO annealed 4H-SiC MOS gated Hall bars are reported in the temperature range 77 K- 423 K. The results indicate higher carrier concentration and lower trapping at increased temperatures, with a clear strong inversion regime at all temperatures. In stark contrast to Si, the Hall mobility increases with temperature for 77 K-373K, above which the mobility decreases slightly. The maximum experimental mobility was found to be ~50 cm 2 V -1 s -1 which is only about 10% of the 4H-SiC bulk mobility indicating that while NO annealing drastically improves trapping, it does not improve the mobility significantly. Supporting modeling results strongly suggest the presence of a disordered SiC channel region.
10
Transition layers at the SiO2∕SiC interface
Tsvetanka Zheleva, Aivars J. Lelis, Gerd Duscher et al. · Applied Physics Letters · 2008 · 154 citations