Japanese Journal of Applied Physics · 1995 · 23 citations · 13 references
EngineeringElectrical EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsIon ImplantationSemiconductor Device MaterialsSilicon MaterialsThin Film AnnealingThin Film Electrical PropertiesThin-film TransistorsActivation EnergyAnnealing EffectsAnnealing Temperature EffectsImplantation Through Thin FilmsInterface Trap DensityPassivationPassivation BehaviorSilicon Thin Films
Fluorine was implanted onto poly-Si films through an oxide layer and its passivation effect on poly-Si films and low-temperature n-ch TFTs was investigated. The implant energy of F + ions was 40 keV, and the F + dose was varied from 5×10 12 to 4×10 15 cm -2 . The fluorine implanted inside poly-Si film preferentially diffused toward the poly- Si/SiO 2 interface during annealing at 600° C. The residual implant damage was found to remain inside poly-Si films after annealing at 600° C when the F + dose was ≥5×10 14 cm -2 . The resistivity and activation energy of the p-type poly-Si resistors were increased as the F + dose increased, resulting from the increase of residual implant damage. However, the characteristics of the n-ch poly-Si TFT were clearly improved when the F + dose was in the range of 5×10 14 to 2×10 15 cm -2 , where the trap state density at the poly Si/SiO 2 interface was found to be reduced because of the passivation effect by fluorine atoms. These results indicated that the fluorine passivation at the poly- Si/SiO 2 interface was effective in an appropriate F + dose range, while the passivation inside the poly-Si film (or grain boundary passivation) was not.
13