IEEE Electron Device Letters · 1985 · 47 citations · 3 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsDopingIii-v SemiconductorsSemiconductor Device MaterialsSemiconductor InterfacesSemiconductor PhysicsSilicon MaterialsElectrical PropertiesJunction FabricationLeakageRapid Thermal AnnealingSilicon AnnealingSilicon DopingThermal AnnealingThermal Annealing Effects
A low temperature method of fabricating conductive (3.5 Ω/ sq.) p <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">+</sup> /n junction diodes possessing excellent <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">I-V</tex> characteristics with reverse-bias leakage less than -3 nA.cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">-2</sup> at -5 V is described. Single crystal n-type 〈100〉 Si is implanted with 60 keV <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">11</sup> B <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">+</inf> through 0.028-µm thick sputtered Ti film. Rapid thermal annealing (RTA) in an N <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</inf> ambient simultaneously forms a 0.36-µm deep p <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">+</sup> /n junction and a 0.063-µm thick bilayer of TiN and TiSi <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</inf> with a resistivity of 22 µΩ.cm. The electrical properties of these diodes are not degraded by annealing for 30 min at 500°C, suggesting that the outer layer of TiN is an effective diffusion barrier between TiSi <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</inf> and Al.
3