IEEE Transactions on Device and Materials Reliability · 2010 · 220 citations · 38 references
EngineeringElectrical EngineeringMaterials ScienceMicroelectronicsSemiconductor DevicesSemiconductor MaterialsDevice CharacterizationDevice ReliabilityMos CapacitorsSemiconductor Device MaterialsSemiconductor ReliabilityWide Band Gap SemiconductorsOxide ReliabilityPower Electronics DevicesReliability Analysis Of Power ElectronicsSiliconSilicon CarbideThermal ActivationTime-dependent Dielectric BreakdownWeibull Model
Silicon carbide’s wide bandgap makes it ideal for high‑temperature applications, yet silicon oxide on SiC is thought to be physically limited at elevated temperatures. The study aims to experimentally assess the long‑term reliability of SiC oxide under high‑temperature stress. Time‑dependent dielectric‑breakdown tests were performed on state‑of‑the‑art 4H‑SiC MOS capacitors and double‑implanted MOSFETs stressed between 225 °C and 375 °C at electric fields of 6–10 MV cm⁻¹. The oxide shows a field‑acceleration factor of ~1.5 dec (MV cm⁻¹)⁻¹, a temperature‑independent activation energy of ~0.9 eV, and area‑dependent Weibull slopes suggesting non‑intrinsic quality, thereby challenging the view that SiC oxide is fundamentally limited by its conduction‑band offset.
The wide-bandgap nature of silicon carbide (SiC) makes it an excellent candidate for applications where high temperature is required. The metal-oxide-semiconductor (MOS)-controlled power devices are the most favorable structure; however, it is widely believed that silicon oxide on SiC is physically limited, particularly at high temperatures. Therefore, experimental measurements of long-term reliability of oxide at high temperatures are necessary. In this paper, time-dependent dielectric-breakdown measurements are performed on state-of-the-art 4H-SiC MOS capacitors and double-implanted MOS field-effect transistors (DMOSFET) with stress temperatures between 225°C and 375°C and stress electric fields between 6 and 10 MV/cm. The field-acceleration factor is around 1.5 dec/(MV/cm) for all of the temperatures. The thermal activation energy is found to be ~ 0.9 eV, independent of the electric field. The area dependence of Weibull slope is discussed and shown to be a possible indication that the oxide quality has not reached the intrinsic regime and further oxide-reliability improvements are possible. Since our reliability data contradict the widely accepted belief that silicon oxide on SiC is fundamentally limited by its smaller conduction-band offset compared with Si, a detailed discussion is provided to examine the arguments of the early predictions.
38
Silicon carbide MEMS for harsh environments
Mehran Mehregany, Christian A. Zorman, N. Rajan et al. · Proceedings of the IEEE · 1998 · 464 citations