Low Resistivity, Thick Heavily Al-Doped 4H-SiC Epilayers Grown by Hot-Wall Chemical Vapor Deposition

Shiyang Ji, Kazutoshi Kojima, Yuuki Ishida, Hidekazu Tsuchida, Sadafumi Yoshida, Hajime Okumura

Materials science forum · 2013 · 24 citations · 7 references

DOIFull text

Open access

Concepts

Abstract

By using hot-wall CVD method, thick heavily Al-doped 4H-SiC epilayers (~90 μm) were grown on 3-inches 4H-SiC wafers. Around the solubility limit, the incorporation behaviors of Al into 4H-SiC were investigated by varying the growth conditions. Among the samples having smooth surfaces, the maximum Al dopants concentration of 3.5×10 20 cm -3 and the minimum resistivity of 16.5 mΩcm were achieved. The results of Hall-effect measurement demonstrate that, along with the increase of Al doping level, the activation ratio of Al dopants gradually increases from several percent up to 100% where the Al dopants concentration is 1.5×10 20 cm -3 .

References

7