Applied Physics Letters · 2008 · 50 citations · 15 references
EngineeringElectrical EngineeringMaterials ScienceElectronic MaterialsMetallurgySemiconductor DevicesChip PackagingMetal-semiconductor ContactsMetalsBrittle FailureBrittle Fracture BehaviorBrittle Fracture TheoryCurrent DensityElectromigrationIntermetallic Compound FormationIntermetallic FormationSoldering
To overcome the effect of current crowding on electromigration-induced pancake-type void formation in flip chip solder joints, two types of Cu column in 90μm flip chip SnAgCu solder joints have been studied. They were (1) the solder contacts the Cu column at bottom and side walls and (2) the solder wets only the bottom surface of the copper column. With a current density of 1.6×104A∕cm2 at 135°C, no failure was detected after 1290h. However, the resistance increased by about 10% due to the formation of a large fraction of intermetallic compounds. We found that electromigration has accelerated the consumption rate of copper column and converted almost the entire solder joint into intermetallic compound. Mechanically, drop impact test indicates a brittle fracture failure in the intermetallic. The electromigration critical product for the intermetallic is discussed.
15
Stress generation by electromigration
I. A. Blech, Conyers Herring · Applied Physics Letters · 1976 · 515 citations
Natural Sciences, Electrical Engineering, Materials Science +16