Journal of Applied Physics · 1988 · 17 citations · 9 references
EngineeringMaterials EngineeringMaterials ScienceSemiconductor DevicesSemiconductor MaterialsThin FilmsCarrier TransportDiffusion In SolidsDopingSemiconductor Device MaterialsThin Film AnnealingThin Film DiffusionAnnealing EffectsDiffusion During AnnealingDiffusion In SemiconductorsDiffusion KineticsDiffusion ProfilesDopant DiffusionRapid Thermal AnnealingThermal Annealing
A new diffusion technique in InP using a Zn3P2 layer as the diffusion source with rapid thermal annealing is evaluated, and a number of interesting features are discussed. A p+ layer can only be achieved at temperatures ranging between 500 and 550 °C with a 15-s minimum diffusion time. Diffusivity is calculated and it is comparable with that of furnace diffusion. However, in order to form a shallow layer, there should not be any high temperature treatment or any other cause for the redistribution of Fe or dopant. Annealing at 850 °C for 15 s prior to diffusion moves the carrier profile from 3000 to 6000 Å deep, and the second diffusion front extends to 2.4 μm for the semi-insulating InP substrate. Similar results are obtained on MOCVD grown semi-insulating Fe:InP epiwafer. Diffusion performed on samples without preannealing resulted in two diffusion fronts and a 2.8-μm deep second diffusion front is observed for a diffusion performed on a preannealed epiwafer.
9
Diffusion profiles of zinc in indium phosphide
B. Tuck, Alan Hooper · Journal of Physics D Applied Physics · 1975 · 120 citations
Double zinc diffusion fronts in InP—Theory and experiment
M. Yamada, P. K. Tien, R. J. Martin et al. · Applied Physics Letters · 1983 · 65 citations