IEEE Transactions on Electron Devices · 2024 · 37 citations · 31 references
EngineeringElectrical EngineeringMaterials ScienceMicroelectronicsSemiconductor DevicesSemiconductor MaterialsDefects In Electronic MaterialsDevice ReliabilityMetal-oxide-semiconductor Field-effect TransistorsSemiconductor DefectsSemiconductor Device MaterialsSemiconductor ReliabilityBias Temperature InstabilityCmos ReliabilityGate DielectricsGate Oxide DegradationPositive Bias Temperature InstabilityReliability DegradationReliability Degradation MechanismsThreshold Voltage
In this work, we demonstrate indium–gallium–zinc oxide (IGZO) transistors fabricated on an 8-in wafer with high uniformity, steep subthreshold slope, and high reliability under positive bias temperature instability (PBTI) stress. The impact of channel compositions, gate dielectrics, and post-treatment conditions on PBTI degradation is systematically characterized and analyzed. The negative threshold voltage ( <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${V}_{\text {TH}}{)}$ </tex-math></inline-formula> shift under positive stress is found to be determined by both hydrogen (H) and oxygen vacancy ( <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$\text{V}_{\text {O}}{)}$ </tex-math></inline-formula> , which is the dominating factor with the highest time exponent in PBTI of IGZO transistors. By reducing H concentration and suppressing <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$\text{V}_{\text {O}}$ </tex-math></inline-formula> generation by process engineering in gate-stack, semiconductor channel, and post-treatment condition, IGZO transistors with high PBTI reliability are demonstrated, achieving a low <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$\vert \Delta {V}_{\text {TH}}\vert $ </tex-math></inline-formula> of 11 mV at 95 °C, <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${V}_{\text {stress}}$ </tex-math></inline-formula> of 3 V ( <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${t}_{\text {ox}}$ </tex-math></inline-formula> = 7 nm, EOT = 3.2 nm by <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${C}$ </tex-math></inline-formula> – <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${V}$ </tex-math></inline-formula> measurements, and <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${E}_{\text {OX}}$ </tex-math></inline-formula> of 3.7 MV/cm), and <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${t}_{\text {stress}}$ </tex-math></inline-formula> of 2 ks.
31
Anderson Janotti, Chris G. Van de Walle · Nature Materials · 2006 · 728 citations
Nanometre-thin indium tin oxide for advanced high-performance electronics
Shengman Li, Mengchuan Tian, Qingguo Gao et al. · Nature Materials · 2019 · 370 citations
Natural Sciences, Materials Engineering, Materials Science +14
Mobility–stability trade-off in oxide thin-film transistors
Yu‐Shien Shiah, Kihyung Sim, Yuhao Shi et al. · Nature Electronics · 2021 · 326 citations
Scaled indium oxide transistors fabricated using atomic layer deposition
Mengwei Si, Zehao Lin, Zhizhong Chen et al. · Nature Electronics · 2022 · 283 citations · Full text