Chemical Vapor Deposition · 2005 · 21 citations · 23 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMaterials ChemistryThin FilmsChemical Vapor DepositionOxide SemiconductorsSemiconductor Thin FilmsThin Film AnnealingThin Film Electrical PropertiesThin-film MaterialsAnnealing Temperature EffectsBreakdown StrengthDielectric ConstantElectrical Breakdown StrengthSiliconSilicon WafersThin Oxide FilmsTitanium Oxides
TiO 2 thin films on silicon wafers have been prepared from the reaction of Ti(NMe 2 ) 4 with O 2 at 250–300 °C by CVD processes. These films, which are carbon free and contain no TiN or TiO x N y species, are amorphous before annealing but crystalline anatase after annealing at 600 °C in air. The average dielectric constant (κ) of the annealed films is 50(5), with an average leakage current of 5(3)×10 –5 A cm –2 , and breakdown strength of 1.8(0.3) MV cm –1 .
23