Journal of The Electrochemical Society · 2003 · 13 citations · 4 references
Natural SciencesMaterials EngineeringMaterials ScienceSurface EngineeringSurface ScienceThin FilmsBarrier PropertiesChemical Vapor DepositionSemiconductor Thin FilmsSilicon MaterialsThin-film DepositionThin-film MaterialsBarrier MaterialsCvd CoatingsNitride Thin FilmsPlasma-enhanced Chemical Vapor DepositionPlasma-enhanced DepositionSilicon CarbideSilicon NitrideThermal Diffusion
We have developed a silicon oxi-carbide and nitride (SiOCNH) barrier film to protect against copper (Cu) thermal diffusion by plasma-enhanced chemical vapor deposition (PECVD) using hexamethyldisiloxane, nitrous oxide <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML1" overflow="scroll"> <mml:mo stretchy="false">(</mml:mo> <mml:msub> <mml:mo>N</mml:mo> <mml:mrow> <mml:mn>2</mml:mn> </mml:mrow> </mml:msub> <mml:mo>O</mml:mo> <mml:mo stretchy="false">)</mml:mo> <mml:mo>,</mml:mo> </mml:math> and ammonia <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML2" overflow="scroll"> <mml:mo stretchy="false">(</mml:mo> <mml:msub> <mml:mo>NH</mml:mo> <mml:mrow> <mml:mn>3</mml:mn> </mml:mrow> </mml:msub> <mml:mo stretchy="false">)</mml:mo> </mml:math> gases. We tried to enhance the Cu barrier property and etching selectivity for low dielectric constant (low- k ) film by adding nitrogen (N) into the barrier silicon oxicarbide (SiOCH) film. The film protects against Cu thermal diffusion at 450°C for 4 h in <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML3" overflow="scroll"> <mml:msub> <mml:mo>N</mml:mo> <mml:mrow> <mml:mn>2</mml:mn> </mml:mrow> </mml:msub> <mml:mo>.</mml:mo> </mml:math> The k value is lower than that for PECVD silicon nitride (SiN) and silicon carbide (SiC) films, but is slightly larger than that of PECVD SiOCH film; it is in the range of 4.17 to 5.21. The leakage current is as low as the value of PECVD SiN film; it is in the range of <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML4" overflow="scroll"> <mml:msup> <mml:mrow> <mml:mn>10</mml:mn> </mml:mrow> <mml:mrow> <mml:mo>−</mml:mo> <mml:mn>9</mml:mn> </mml:mrow> </mml:msup> </mml:math> to <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML5" overflow="scroll"> <mml:msup> <mml:mrow> <mml:mn>10</mml:mn> </mml:mrow> <mml:mrow> <mml:mo>−</mml:mo> <mml:mn>10</mml:mn> </mml:mrow> </mml:msup> <mml:mo>A</mml:mo> <mml:mo>/</mml:mo> <mml:msup> <mml:mi mathvariant="normal">cm</mml:mi> <mml:mrow> <mml:mn>2</mml:mn> </mml:mrow> </mml:msup> </mml:math> at 1 MV/cm. This value decreases with increasing <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML6" overflow="scroll"> <mml:msub> <mml:mo>NH</mml:mo> <mml:mrow> <mml:mn>3</mml:mn> </mml:mrow> </mml:msub> </mml:math> flow rate. However, Cu thermal diffusion increased with increasing <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML7" overflow="scroll"> <mml:msub> <mml:mo>NH</mml:mo> <mml:mrow> <mml:mn>3</mml:mn> </mml:mrow> </mml:msub> </mml:math> flow rate. The diffusion depth is less than 20 nm. The diffusion behavior can be explained by the result that diffusion is controlled by the small pore size, high density, and small compressive stress in SiOCNH film. The average pore size is smaller than 0.49 nm, which is generally smaller than that of SiOCH film deposited using <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML8" overflow="scroll"> <mml:msub> <mml:mo>N</mml:mo> <mml:mrow> <mml:mn>2</mml:mn> </mml:mrow> </mml:msub> <mml:mo>O</mml:mo> </mml:math> gas. The film density is greater than 2.14 g/cm 3 , which is larger than that of SiOCH film. The etching selectivity to silicon oxide deposited by PECVD using tetraethoxysilane (PECVD tetraethylorthosiloxane, TEOS <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML9" overflow="scroll"> <mml:msub> <mml:mi mathvariant="normal">SiO</mml:mi> <mml:mrow> <mml:mn>2</mml:mn> </mml:mrow> </mml:msub> <mml:mo stretchy="false">)</mml:mo> </mml:math> film is ∼15. The dynamic hardness is almost the same as the value of quartz and is 2.0 to 2.5 times larger than the value of PECVD TEOS <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML10" overflow="scroll"> <mml:msub> <mml:mi mathvariant="normal">SiO</mml:mi> <mml:mrow> <mml:mn>2</mml:mn> </mml:mrow> </mml:msub> </mml:math> film. The Young’s modulus was ∼2.0 and 2.5 times larger than the values of quartz and PECVD TEOS <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML11" overflow="scroll"> <mml:msub> <mml:mi mathvariant="normal">SiO</mml:mi> <mml:mrow> <mml:mn>2</mml:mn> </mml:mrow> </mml:msub> </mml:math> film, respectively. The adhesion strength on Cu is the same as that of PECVD SiOCH film and slightly smaller than that of PECVD SiN film. The desorption of ammonium <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline" id="ML12" overflow="scroll"> <mml:mo stretchy="false">(</mml:mo> <mml:msubsup> <mml:mo>NH</mml
4
Jun Magoshi, Michio Mizuide, Yoshiko Magoshi et al. · Journal of Polymer Science Polymer Physics Edition · 1979 · 118 citations
Ryoichi Suzuki, Toshiyuki Ohdaira, Yoshimi Shioya et al. · Japanese Journal of Applied Physics · 2001 · 30 citations