Japanese Journal of Applied Physics · 2000 · 330 citations · 17 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsIii-v SemiconductorsSemiconductor Crystal GrowthSemiconductor DefectsSemiconductor HeterostructuresWide Band Gap SemiconductorsWide-bandgap SemiconductorsCrack FormationCracksGallium NitrideGallium Nitride (Gan) MaterialsLattice ReductionMetalorganic Chemical Vapor DepositionMetalorganic Vapor Phase EpitaxyThermal Mismatch
We present a simple method for the elimination of cracks in GaN layers grown on Si (111). Cracking of GaN on Si usually occurs due to large lattice and thermal mismatch of GaN and Si when layer thicknesses exceeds approximately 1 µm. By introducing thin, low-temperature AlN interlayers, we could significantly reduce the crack density of the GaN layer. The crack density is practically reduced to zero from an original crack density of 240 mm -2 corresponding to crack-free regions of 3×10 -3 mm 2 . Additionally for the GaN layer with low temperature interlayers, the full width at half maximum X-ray (2024) rocking curve is improved from approximately 270 to 65 arcsec.
17
Stress evolution during metalorganic chemical vapor deposition of GaN
Sean Hearne, Eric Chason, Jung Han et al. · Applied Physics Letters · 1999 · 243 citations
Natural Sciences, Materials Engineering, Materials Science +17