2005 · 28 citations · 6 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsMicrofabricationSemiconductor DevicesChip PackagingMems PackagingPackaging EngineeringPackaging MaterialsWafer BondingBond DegradationBonding TechniquesBonding Temperature EffectsDegradationFlip-chip BondingPackaging ApplicationsTransient Liquid Phase BondingWafer-to-wafer Bonding
This paper explores the use of transient liquid phase bonding for microsystem packaging applications. Two types of bonds are demonstrated: a thin-film evaporated indium-gold bond and an electroplated nickel-tin bond. Both bonds are formed at 300/spl deg/C for about 1.5 hours in a conventional wafer bonder. The wafers were heated to over 400 /spl deg/C for more than an hour after bonding without any signs of bond degradation. The indium-gold bond demonstrated good electrical contact, but poor permeability performance. However, the nickel-tin bond was void free and sealed cavities with bond ring widths as little as 50 /spl mu/m. The cross section of the nickel-tin TLP bond was analyzed with EDAX software to verify the formation of intermetallic compounds.
6
Integrated sensor wafer-level packaging
S.A. Audet, K. M. Edenfeld · 2002 · 37 citations
From zero- to second-level packaging of RF-MEMS devices
Anne Jourdain, Kristof Vaesen, Jennifer Scheer et al. · 2005 · 30 citations