EngineeringElectrical EngineeringMaterials ScienceElectronic MaterialsMicroelectronicsSemiconductor DevicesMetal-oxide-semiconductor Field-effect TransistorsMicrowave Semiconductor DevicesPlasma-surface InteractionsSemiconductor Device MaterialsSemiconductor InterfacesSilicon MaterialsFabricationInterface TrapsOxidationPlasma OxidationPlasma-assisted OxidationPlasma-enhanced OxidationSilicon Carbide (Sic) MaterialsTraps
The microwave plasma oxidation under the relatively high pressure (6 kPa) region is introduced into the fabrication process of SiO 2 /4H-SiC stack. By controlling the oxidation pressure, species, and temperature, the record low density of interface traps (∼ 4 × 10 10 cm −2 ⋅eV −1 @ E c − 0.2 eV) is demonstrated on SiO 2 /SiC stack formed by microwave plasma oxidation. And high quality SiO 2 with very flat interface (0.27-nm root-mean-square roughness) is obtained. High performance SiC metal–oxide–semiconductor field-effect transistors (MOSFETs) with peak field effect mobility of 44 cm −2 ⋅eV −1 is realized without additional treatment. These results show the potential of a high-pressure plasma oxidation step for improving the channel mobility in SiC MOSFETs.
28