40 $\mu{\rm m}$ Flip-Chip Process Using Ag–In Transient Liquid Phase Reaction

Wen P. Lin, Chu-Hsuan Sha, Chin C. Lee

IEEE Transactions on Components Packaging and Manufacturing Technology · 2012 · 26 citations · 8 references

Concepts

Abstract

A flip-chip interconnect process at 180 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">°</sup> C using the silver-indium (Ag-In) binary system is reported. An array of 50 × 50 flip-chip joints with 100 μm pitch and 40 μm joint diameter was fabricated. Each joint has the column structure of Ag/(Ag)/Ag <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> In/(Ag) that connects the silicon (Si) chip to the copper (Cu) substrate. The joint height is approximately 50 μm. In this structure, Ag <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> In is a dominating intermetallic compound in the Ag-In system with melting temperature of 660 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">°</sup> C. (Ag) is a solid solution phase of Ag with In composition up to 20 at.%. It has a solidus temperature range of 695 to 962 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">°</sup> C depending on In composition. In long-term operation, (Ag)/Ag <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> In/(Ag) is expected to gradually convert to a single (Ag) phase, which is more reliable. Thus, the flip-chip joints will get better in use. In fabrication, 50 × 50 Ag columns were made on Si wafer coated with chromium (Cr) and gold (Au). The Cu substrate was electroplated with Ag(10 μm)/In(5 μm)/Ag(thin). Si chips with Ag columns were bonded to Cu substrates at 180 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">°</sup> C for 5 min. No flux was used. Cross-sectional scanning electron microscopy images show that all 50 Ag columns in one row are well bonded to the Cu substrate without visible voids or cracks. Energy-dispersive X-ray spectroscopy data indicate that the resulting column structure is Ag/(Ag)/Ag <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> In/(Ag). The process temperature of this new interconnect method is 80 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">°</sup> C below the typical reflow temperature of tin-based lead-free solders.

References

8