Japanese Journal of Applied Physics · 1995 · 12 citations · 8 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsSurface ScienceCarrier TransportDopingSemiconductor PhysicsSemiconductor SurfacesSurface DiffusionSurface PhysicsAnnealing Time EffectsCarrier ConcentrationDiffusion During AnnealingDiffusion ProfilesDoped SemiconductorsDoping ProfilesGaussian DistributionsSilicon Doping
The behavior of active and inactive boron produced by vapor-phase doping during subsequent hydrogen annealing is investigated. In samples doped at 800° C, there is a great deal of inactive boron at the surface, which gives an exponential profile just after doping. For these samples, fast out-diffusion of inactive boron is observed during subsequent hydrogen annealing at 800° C. After 20 min of subsequent annealing, almost all of the inactive boron diffuses out and the sheet boron concentration becomes identical to the carrier concentration. The out-diffusion of inactive boron does not follow a Gaussian distribution. In samples doped at 900° C, almost complete activation is achieved just after doping. The diffusion of active boron during subsequent annealing can be described as Gaussian: the surface carrier concentration decreases in proportion to the square root of the annealing time. This behavior is not affected by the existence of inactive boron.
8
Ichiro Mizushima, Atsushi Murakoshi, Masaharu Watanabe et al. · Japanese Journal of Applied Physics · 1994 · 37 citations