Applied Physics Letters · 2003 · 39 citations · 12 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsInterface ScienceSemiconductor DevicesDielectricsElectrical ConductivityElectrode MaterialsInterconnect TechnologySemiconductor ReliabilityActivation EnergyCopper InterconnectsCurrent DensityElectromigrationElectromigration ReliabilityExtrusionInterconnect MaterialsInterconnect Reliability
Electromigration (EM) reliability was investigated for Cu/porous low k interconnects. The porous low k dielectric was a methylsilsesquioxane (MSQ) based spin-on organosilicate material with k of 2.2. The activation energy for EM failure was found to be about 0.9 eV for Cu/porous MSQ between 208 and 367 °C, which is commonly associated with mass transport at the Cu/SiNx cap-layer interface. The threshold product of current density and line length (jL)c for Cu/porous MSQ was found to be 2500–3000 A/cm. The reduction in EM lifetime compared with Cu/oxide interconnect can be attributed to smaller back stress, due to less thermomechanical confinement of Cu/low k interconnects. Most interconnects failed by voiding at the cathode. Some lateral Cu extrusion followed by interfacial breakdown was also observed near the anode.
12
Stress evolution due to electromigration in confined metal lines
M. A. Korhonen, P. Bo rgesen, K. N. Tu et al. · Journal of Applied Physics · 1993 · 733 citations
Electromigration path in Cu thin-film lines
C.‐K. Hu, R. Rosenberg, K. Y. Lee · Applied Physics Letters · 1999 · 329 citations
Natural Sciences, Materials Engineering, Materials Science +17