Journal of Applied Physics · 1983 · 50 citations · 14 references
EngineeringElectrical EngineeringMaterials ScienceElectronic MaterialsRadiation PhysicsSemiconductor DevicesDopingIon ImplantationRadiation Damage In MaterialsSemiconductor Device MaterialsSemiconductor InterfacesSemiconductor ReliabilityAnnealing Temperature EffectsAnnealing Time EffectsDopant ActivationDopant DiffusionImplantation-induced Defect FormationPenetration DepthRadiation-enhanced DiffusionSemiconductor Doping Profiles
The minimum annealing time for complete dopant activation of ion implant doses of 2.8×1014 and 2.8×1015 B+/cm2 are found for temperatures ranging from 850 to 1100 °C. For samples annealed at 1100 °C for 10 s and 1000 °C for 15 min electrical characteristics of diodes are correlated with dopant profiles and penetration depth of transmission electron microscope observable defects. Radiation-enhanced diffusion, associated with the ion implant damage, is the major contributor to dopant diffusion for 10-s anneals at 1100 °C. The junction depth produced by annealing for 10 s at 1100 °C is significantly less than that produced by annealing for 15 min at 1000 °C, while the electrical characteristics of the diodes are the same.
14
Laser and Electron Beam Interactions with Solids
N. Bloembergen, B. R. Appleton, G. K. Celler · MRS Bulletin · 1982 · 588 citations · Full text
Physical and electrical properties of laser-annealed ion-implanted silicon
A. Gat, J. F. Gibbons, T. J. Magee et al. · Applied Physics Letters · 1978 · 173 citations