physica status solidi (b) · 2001 · 209 citations · 122 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsDislocations In SemiconductorsEpitaxial GrowthIii-v SemiconductorsSemiconductor DefectsWide Band Gap SemiconductorsWide-bandgap SemiconductorsDislocations In Epitaxial FilmsEpitaxial Growth Of Wide-bandgap SemiconductorsEpitaxial Lateral OvergrowthGallium Nitride (Gan) MaterialsGallium Nitride Crystal GrowthPhotoluminescencePhotoluminescence Spectroscopy
GaN devices depend on heteroepitaxy onto sapphire or 6H‑SiC because bulk GaN crystals are unavailable, but this introduces threading dislocations of three types that degrade device quality. Epitaxial lateral overgrowth reduces threading dislocation density to ~10⁶ cm⁻², narrows near‑bandgap photoluminescence to <1 meV, and lowers deep electron trap density to <10¹⁴ cm⁻³ compared with standard GaN.
Since there is no GaN bulk single crystal available, the whole technological development of GaN based devices relies on heteroepitaxy. Numerous defects are generated in the heteroepitaxy of GaN on sapphire or 6H-SiC, mainly threading dislocations (TDs). Three types of TDs are currently observed, a type (with Burgers vector 1/3〈〉); c type (with 〈0001〉) and mixed a+c (1/3〈〉). The Epitaxial Lateral Overgrowth (ELO) technology produces high quality GaN with TD densities in the mid 106 cm—2, linewidth of the low-temperature photoluminescence (PL) near-bandgap recombination peaks <1 meV and deep electron traps reduced below 1014 cm—3 (compared to mid 1015 cm—3 in standard GaN). Numerous modifications of the ELO process have been proposed in order either to avoid technological steps (mask-less ELO) or to improve it (pendeo-epitaxy). Basically developed on either sapphire or 6H-SiC, the ELO technology is also achievable on (111)Si or (111)3C-SiC/Si provided that an appropriate buffer layer is grown to avoid cracks. More sophisticated technologies have been implemented to further increase the useable part of the ELO GaN surface (two technological steps, three-step ELO). Unfortunately, in-depth understanding of the basic ELO process is still missing, i.e. of the growth anisotropy and bending of dislocations.
122
Shuji Nakamura, Masayuki Senoh, Shin‐ichi Nagahama et al. · Applied Physics Letters · 1998 · 732 citations