Hybrid Circuits · 1994 · 10 citations · 4 references
EngineeringElectrical EngineeringMaterials ScienceMicroelectronicsSemiconductor DevicesSemiconductor MaterialsChip PackagingIntegrated Circuit DesignSemiconductor Device MaterialsSemiconductor InterfacesSemiconductor SurfacesWafer BondingDeformationFlip-chip BondingFlip-chip BumpingFlip-chip PackagingProcess ParametersProcess Parameters OptimizationSilicon WafersWire Bonding
Ball-bumping is a flexible low cost bumping technology based on the conventional wire bonding procedure. It is applicable to single chips or whole wafers as well as to substrates. As established wire-bonding machines can be used, expensive bumping-process equipment for phototooling and plating is not necessary. Flip-chip bonding is the most advantageous attach method of high frequency applications. Compared with wire-bonding and TAB it allows the highest contact density, the shortest signal paths and lowest interconnection parasitics. The reduced pad sizes and pitches, not only of GaAs devices, demand a well controlled bump deformation during flip-chip bonding. This work develops process parameters for the flip-chip bonding of silicon and GaAs devices with respect to the best interconnection result by lowest bonding force and ball-bump deformation. Ball-bumps with diameters of 50 and 80 urn (2.0 and 3.2 mils) were created using 98% AuPd bump wire with diameters of 18 µm (0.7 mil) and 25 µm (1.0 mil) respectively. Ball-bumping with a minimal pitch of 70 µm (2.8 mils) has been achieved. A special preparation allowed the shear test investigation of each bump/pad interface after flip-chip attach. Bonding forces of 20 and 25 cN/bump respectively lead to a good welding in the bump/substrate interface due to the special shape of ball-bumps. For silicon devices which have a pad metallisation of aluminium, the shear forces of the bump/pad interface increase after flip-chip bonding, too. No cratering of GaAs and silicon occurs after flip-chip bonding due to a low bonding force ramp of 5 cN/s and 10 cN/s respectively. The flip-chip attach of a Fujitsu FLR 016 GaAs-FET which has pad sizes of 35 urn is demonstrated. In this case, substrate bumping is the more advantageous bumping method. The feasibility of fine-pitch TAB attach using ball-bumps is introduced. 100 µm (3.9 mils) pitch silicon devices with 328 pads were ball-bumped for both solder and thermal-compression TAB. Bond forces were in the range of 9–11 cN/bump and 15–21 cN/bump respectively. Pull forces of approximately 30 cN/lead show good results of the bump/lead interconnection after TAB.
4
Electroless deposition of bumps for TAB technology
J. Simon, E. Zakel, H. Reichl · 2002 · 46 citations
Natural Sciences, Materials Engineering, Materials Science +12
A Stud-bump-bonding Technique For High Density Multi-chip-module
Y. Bessho, Y. Tomura, Y. Hakotani et al. · 2005 · 25 citations