Surface and Interface Analysis · 2010 · 24 citations · 19 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsDevice CharacterizationSemiconductor Device MaterialsSemiconductor InterfacesSemiconductor PhysicsSemiconductor SurfacesSemiconductor Thin FilmsInterface DensityInterface StatesJunction Ideality FactorMagnetron SputteringSchottky Barrier DiodesSchottky BarriersSemiconductor CharacterizationSeries Resistance
Abstract The purpose of this study is to analyze interface states ( N ss ) in Au/TiO 2 (Rutile)/n–Si Schottky barrier diodes (SBDs). TiO 2 was deposited on a n–Si substrate by reactive magnetron sputtering and annealed at 900 °C for 4 h in atmosphere to obtain rutile phase. The current voltage (I‐V) characteristics of SBDs were measured at room temperature. From the I‐V characteristics of the SBDs ideality factor ( n ) and zero‐bias barrier height values (ϕ Bo ) 2.3 and 0.76 eV, respectively, were obtained. The N ss distribution profile ( N ss ) as a function of ( E c − E ss ) was extracted from the forward‐bias I‐V measurements by taking account effective barrier height and (ϕ e ) and series resistance ( R s ) for the Schottky diode. N ss values ranges from 4.3 × 10 12 cm −2 eV −1 in ( E c − 0.33) eV and 8.0 × 10 13 cm −2 eV −1 in ( E c − 0.33) eV. These values are better than in the literature values where TiO 2 was deposited sol‐gel method. The N ss values taking into R s were lower than without R s . This shows that R s should be taking account. Copyright © 2010 John Wiley & Sons, Ltd.
19
Barrier inhomogeneities at Schottky contacts
J.H. Werner, H. Güttler · Journal of Applied Physics · 1991 · 1.6K citations
Rutile-type TiO2 thin film for high-k gate insulator
Masaru Kadoshima, Masahiko Hiratani, Yasuhiro Shimamoto et al. · Thin Solid Films · 2003 · 244 citations
Natural Sciences, Materials Engineering, Materials Science +14