Micromachines · 2020 · 42 citations · 45 references
Natural SciencesMaterials EngineeringMaterials ScienceMicroelectromechanical SystemsSurface ScienceThin FilmsMicrofabrication MaterialsThin-film MaterialsVacuum PackagingWafer BondingFilm ThicknessPlasmonic Thin FilmsSilicon WafersSilicon-to-glass BondingSurface Roughness ParametersWafer-to-wafer Bonding
Au-Au surface activated bonding (SAB) using ultrathin Au films is effective for room-temperature pressureless wafer bonding. This paper reports the effect of the film thickness (15-500 nm) and surface roughness (0.3-1.6 nm) on room-temperature pressureless wafer bonding and sealing. The root-mean-square surface roughness and grain size of sputtered Au thin films on Si and glass wafers increased with the film thickness. The bonded area was more than 85% of the total wafer area when the film thickness was 100 nm or less and decreased as the thickness increased. Room-temperature wafer-scale vacuum sealing was achieved when Au thin films with a thickness of 50 nm or less were used. These results suggest that Au-Au SAB using ultrathin Au films is useful in achieving room-temperature wafer-level hermetic and vacuum packaging of microelectromechanical systems and optoelectronic devices.
45
Bonding of silicon wafers for silicon-on-insulator
W. Maszara, Georges Goetz, A.L. Caviglia et al. · Journal of Applied Physics · 1988 · 861 citations
Review Article: Stress in thin films and coatings: Current status, challenges, and prospects
G. Abadias, Eric Chason, Jozef Kečkéš et al. · Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · 2018 · 820 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +17