Passivation of Thin Channel Zinc Tin Oxide TFTs Using Al<sub>2</sub>O<sub>3</sub> Deposited by O<sub>3</sub>-Based Atomic Layer Deposition

Christopher Allemang, Rebecca L. Peterson

IEEE Electron Device Letters · 2019 · 27 citations · 30 references

Concepts

Abstract

Here, we fabricate solution processed zinc tin oxide bottom gate top contact thin film transistors (TFTs) with active layer thickness down to 6 nm by varying the solution molarity and number of layers. As-fabricated devices show hysteresis as large as 12.65 V. The hysteresis is then studied under vacuum to understand the important role of the back channel in electrical performance. After vacuum treatment, the hysteresis measured under vacuum was reduced to -0.05 V. Alumina deposited on the back channel using atomic layer deposition (ALD) is used for passivation. The TFTs passivated with an H <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> O-based ALD process show conductive behavior after passivation while an O <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> -based ALD process results in a negative threshold voltage shift dependent on the thickness of the active layer. O <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> -based passivated devices show good stability with a field effect mobility of 8.3 cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sup> V <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">-1</sup> s <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">-1</sup> , V <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">t</sub> of 5.5 V, and hysteresis of 0.85 V.

References

30