Comparison of thermal and plasma-enhanced atomic layer deposition of niobium oxide thin films

Saravana Balaji Basuvalingam, Bart Macco, Harm C. M. Knoops, Jimmy Melskens, W. M. M. Kessels, Ageeth A. Bol

Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · 2018 · 35 citations · 39 references

DOIFull text

Open access

Concepts

Abstract

Niobium pentoxide was deposited using tBuN=Nb(NEt2)3 as niobium precursor by both thermal atomic layer deposition (ALD) and plasma-enhanced atomic layer deposition (PE-ALD) with H2O and O2 plasma as coreactants, respectively. The deposition temperature was varied between 150 and 350 °C in both ALD processes. Amorphous films were obtained in all cases. Self-limiting saturated growth was confirmed for both ALD processes along with high uniformity over a 200 mm Si wafer. The PE-ALD process enabled a higher growth per cycle (GPC) than the thermal ALD process (0.56 Å vs 0.38 Å at 200 °C, respectively), while the GPC decreases with increasing temperature in both cases. The high purity of the film was confirmed using Rutherford backscattering spectrometry, elastic recoil detection, and x-ray photoelectron spectroscopy, while the latter technique also confirmed the Nb+5 oxidation state of the niobium oxide films. The thermal ALD deposited films were substoichiometric due to the presence of oxygen vacancies (VO), of which a more dominant presence was observed with increasing deposition temperature. The PE-ALD deposited films were found to be near stoichiometric for all investigated deposition temperatures.

References

39