Chinese Physics B · 2013 · 24 citations · 11 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsInterface ScienceSurface ScienceAtomic Layer DepositionInterface EngineeringOxide SemiconductorsSemiconductor InterfacesSemiconductor SurfacesThin-film MaterialsAnnealingAnnealing EffectsAnnealing Temperature EffectsAnnealing Time EffectsAtomic Layer Deposition InterfacesGrazing-incidence X-ray DiffractionInterface CharacterizationInterface States
High-temperature annealing of the atomic layer deposition (ALD) of Al2O3 films on 4H-SiC in O2 atmosphere is studied with temperature ranging from 800 °C to 1000 °C. It is observed that the surface morphology of Al2O3 films annealed at 800 °C and 900 °C is pretty good, while the surface of the sample annealed at 1000 °C becomes bumpy. Grazing incidence X-ray diffraction (GIXRD) measurements demonstrate that the as-grown films are amorphous and begin to crystallize at 900 °C. Furthermore, C—V measurements exhibit improved interface characterization after annealing, especially for samples annealed at 900 °C and 1000 °C. It is indicated that high-temperature annealing in O2 atmosphere can improve the interface of Al2O3/SiC and annealing at 900 °C would be an optimum condition for surface morphology, dielectric quality, and interface states.
11
Oxygen deficiency defects in amorphous Al2O3
Timofey V. Perevalov, O. E. Tereshenko, V. A. Gritsenko et al. · Journal of Applied Physics · 2010 · 118 citations