IEEE Transactions on Advanced Packaging · 2004 · 21 citations · 12 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMetallic MaterialsMetallurgyAlloysMetalsPlasma-surface InteractionsBumpsDuctile FractureFlip-chip BumpingFlip-chip PackagingFracture Initiation In Ductile MaterialsInterface Shear StrengthPlasma-assisted BondingSoldering
A new flux-free reflow process using Ar+10%H/sub 2/ plasma was investigated for application to solder bump flip chip packaging. The 100-/spl mu/m diameter Sn-3.5wt%Ag solder balls were bonded to 250-/spl mu/m pitch Cu/Ni under bump metallurgy (UBM) pattern by laser solder ball bonding method. Then, the Sn-Ag solder balls were reflowed in Ar+H/sub 2/ plasma. Without flux, the wetting between solder and UBM occurred in Ar+H/sub 2/ plasma. During plasma reflow, the solder bump reshaped and the crater on the top of bump disappeared. The bump shear strength increased as the Ni/sub 3/Sn/sub 4/ intermetallic compounds formed in the initial reflow stage but began to decrease as coarse (Cu,Ni)/sub 6/Sn/sub 5/ grew at the solder/UBM interface. As the plasma reflow time increased, the fracture mode changed from ductile fracture within the solder to brittle fracture at the solder/UBM interface. The off-centered bumps self-aligned to patterned UBM pad during plasma reflow. The micro-solder ball defects occurred at high power prolonged plasma reflow.
12
G.W.A.D. · Microelectronics Reliability · 1990 · 289 citations
Fluxless soldering in air and nitrogen
N. Koopman, Stephen M. Bobbio, S. Nangalia et al. · 2002 · 34 citations