2003 · 15 citations · 5 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMaterials CharacterizationMetallic MaterialsAlloysMetalsPhysical MetallurgyDifferential CalorimetryEnergy-dispersive X-ray SpectroscopyFatigue Crack GrowthFatigue Crack InitiationGrain Boundary MigrationGrain Boundary SlidingJoint ReliabilitySoldering
The solder interaction of Pb within the Sn/Ag/Cu system was characterized using Differential Scanning Calorimetry (DSC). Components were then assembled with the Pb-free solder. Cross-sectioning and fine polishing were performed on the solder joints at the as-soldered stage and after temperature cycle readouts at 250, 500, 750, and 1000 cycles. The microstructure of the solder joints was examined using Scanning Electron Microscopy (SEM), and solder elements were mapped and identified by Energy-Dispersive X-ray (EDX) analysis. DSC detected Pb reaction with Sn/Ag at 179/spl deg/C and ternary compound formation. SEM/EDX found that Pb diffused into the Sn/Ag/Cu matrix during reflow soldering to form different microstructures, namely CuSn, SnAg, SnPbAg, and Pb-rich phases. The SnAg structure was found as a rod/needle morphology that was detrimental to solder joint reliability. During temperature cycling, this structure loosened its embedding effects due to grain-boundary sliding in the solder matrix, which accelerated solder fatigue crack propagation. Solutions to this problem are discussed.
5
Interfacial reaction studies on lead (Pb)-free solder alloys
S. K. Kang, Da‐Yuan Shih, K. Fogel et al. · 2002 · 25 citations
Natural Sciences, Materials Engineering, Materials Science +17
Microstructural coarsening of lead free solder joints during thermal cycling
Li-Lei Ye, Zonghe Lai, Joe Liu et al. · 2002 · 24 citations
Natural Sciences, Materials Engineering, Materials Science +17
An intermetallic study of solder joints with Sn-Ag-Cu lead-free solder
Chien-Feng Chan, S. K. Lahiri, Peng Yuan et al. · 2002 · 14 citations
Natural Sciences, Materials Engineering, Materials Science +15