Journal of Applied Physics · 1987 · 11 citations · 17 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsThin FilmsAmorphous MaterialsAmorphous SolidsChemical Vapor DepositionCrystallization ProcessesGrain GrowthSilicon MaterialsAmorphous Semiconductor FilmsFilm ThicknessHall EffectLow-pressure Chemical Vapor DepositionPost-implantation AnnealingRapid Thermal AnnealingSheet ResistanceThermal Annealing
Amorphous Si films of 4000 Å were deposited using low-pressure chemical-vapor deposition and implanted with arsenic or boron at doses of 5×1013, 5×1014, and 5×1015 cm−2. These films were then rapid thermally annealed (RTA) using an Eaton Nova ROA-400 system at temperatures ranging from 900 to 1200 °C and dwell times ranging from 1 to 30 s. It was found that grain growth initiated very rapidly (less than 2 s at 1100 °C). Grain growth saturation (when grain size equals the film thickness) was reached in 5×1015 dose samples after a 1200 °C, 10-s RTA. The sheet resistance decreased with increasing RTA temperature and dwell time. Hall mobility increased with both RTA temperature and time. The temperature coefficient of resistance (TCR) was negative at low dose implants and became positive at higher dose implants. The lowest TCR was found in films implanted with medium dose. In general, 1200 °C/10-s RTA is an optimal condition for crystallization and annealing of the 5×1015 and 5×1014 cm−2 dose films while longer times are necessary for the 5×1013 cm−2 dose films.
17
Hall Mobility in Chemically Deposited Polycrystalline Silicon
T. I. Kamins · Journal of Applied Physics · 1971 · 434 citations
Dopant segregation in polycrystalline silicon
Mohammad M. Mandurah, Krishna C. Saraswat, C. R. Helms et al. · Journal of Applied Physics · 1980 · 371 citations