Low-temperature SiO2 growth using fluorine-enhanced thermal oxidation

Mizuho Morita, S. Aritome, M. Tsukude, Takao MURAKAWA, M. Hirose

Applied Physics Letters · 1985 · 19 citations · 6 references

Concepts

Abstract

A new low-temperature oxidation technique of silicon to obtain high quality Si-SiO2 interface and bulk SiO2 layer is presented. A few tens-nanometer-thick oxide layers are grown within 30 min at temperatures between 600 and 800 °C by fluorine-enhanced thermal oxidation using an O2+NF3 gas mixture. Fluorine atoms incorporated in the oxide layer are substituted by oxygen atoms through post-annealing in pure oxygen gas at the same temperature as oxidation. An interface state density as low as 2×1010 cm−2 eV−1 near midgap is achieved for oxides grown at 800 °C and 8×1010 cm−2 eV−1 even for oxides at 600 °C. The dielectric breakdown strength of the oxide is improved by the post-annealing in O2.