Electrical characterization of amorphous lanthanum aluminate thin films grown by molecular-beam deposition on silicon

L. F. Edge, Darrell G. Schlom, P. Sivasubramani, Robert M. Wallace, B. Holländer, J. Schubert

Applied Physics Letters · 2006 · 57 citations · 22 references

Concepts

Abstract

Amorphous LaAlO3 thin films were deposited at room temperature directly on n-type and p-type Si (001) by molecular beam deposition. The dielectric properties of the stoichiometric amorphous LaAlO3 thin films deposited on silicon were determined through capacitance-voltage and current-voltage measurements. The electrical measurements indicate that the amorphous LaAlO3 thin films have a dielectric constant (K) of K=16±2. This is significantly lower than the K=24 of crystalline LaAlO3. The equivalent oxide thickness values range between 9.8 and 15.5Å for films deposited on n-type silicon with physical thicknesses of 45–75Å.

References

22