Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · 2014 · 46 citations · 33 references
EngineeringMaterials EngineeringMaterials ScienceSemiconductor DevicesSemiconductor MaterialsThin FilmsAtomic Layer DepositionMos CapacitorsSemiconductor Device MaterialsSemiconductor InterfacesSemiconductor Thin FilmsThin Film Electrical PropertiesAnnealingCapacitance-voltage CharacteristicsCapacitance-voltage CharacterizationElectrical PropertiesLeakage CurrentPlasma-enhanced Atomic Layer DepositionPlasma-enhanced DepositionSilicon Wafers
Ga2O3 dielectric thin films were deposited on (111)-oriented p-type silicon wafers by plasma-enhanced atomic layer deposition using trimethylgallium and oxygen plasma. Structural analysis of the Ga2O3 thin films was carried out using grazing-incidence x-ray diffraction. As-deposited films were amorphous. Upon postdeposition annealing at 700, 800, and 900 °C for 30 min under N2 ambient, films crystallized into β-form monoclinic structure. Electrical properties of the β-Ga2O3 thin films were then investigated by fabricating and characterizing Al/β-Ga2O3/p-Si metal–oxide-semiconductor capacitors. The effect of postdeposition annealing on the leakage current densities, leakage current conduction mechanisms, dielectric constants, flat-band voltages, reverse breakdown voltages, threshold voltages, and effective oxide charges of the capacitors were presented. The effective oxide charges (Qeff) were calculated from the capacitance–voltage (C-V) curves using the flat-band voltage shift and were found as 2.6 × 1012, 1.9 × 1012, and 2.5 × 1012 cm−2 for samples annealed at 700, 800, and 900 °C, respectively. Effective dielectric constants of the films decreased with increasing annealing temperature. This situation was attributed to the formation of an interfacial SiO2 layer during annealing process. Leakage mechanisms in the regions where current increases gradually with voltage were well fitted by the Schottky emission model for films annealed at 700 and 900 °C, and by the Frenkel–Poole emission model for film annealed at 800 °C. Leakage current density was found to improve with annealing temperature. β-Ga2O3 thin film annealed at 800 °C exhibited the highest reverse breakdown field value.
33
Large-size β-Ga2O3 single crystals and wafers
Encarnación G. Vı́llora, Kiyoshi Shimamura, Yukio Yoshikawa et al. · Journal of Crystal Growth · 2004 · 633 citations
Natural Sciences, Materials Engineering, Materials Science +12
Takayoshi Oshima, Takeya Okuno, Shizυo Fujita · Japanese Journal of Applied Physics · 2007 · 558 citations
Ga2O3 films for electronic and optoelectronic applications
M. Passlack, E. Fred Schubert, W. S. Hobson et al. · Journal of Applied Physics · 1995 · 434 citations