Chinese Physics Letters · 2018 · 14 citations · 23 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsChemical Vapor DepositionDefects In Electronic MaterialsSemiconductor DefectsSemiconductor ReliabilityStacking FaultsWide-bandgap SemiconductorsCarrier LifetimeCarrier Lifetime MeasurementDevice DegradationPhotoconductivityPhotoluminescencePhotoluminescence SpectroscopySilicon CarbideSilicon Carbide (Sic) Materials
Effect of triangle structure defects in a 180-μm-thick as-grown n-type 4H-SiC homoepitaxial layer on the carrier lifetime is quantitatively analyzed, which is grown by a horizontal hot-wall chemical vapor deposition reactor. By microwave photoconductivity decay lifetime measurements and photoluminescence measurements, the results show that the average carrier lifetime of as-grown epilayer across the whole wafer is 2.59 μs, while it is no more than 1.34 μs near a triangle defect (TD). The scanning transmission electron microscope results show that the triangle structure defects have originated from 3C-SiC polytype and various types of as-grown stacking faults. Compared with the as-grown stacking faults, the 3C-SiC polytype has a great impact on the lifetime. The reduction of TD is essential to increasing the carrier lifetime of the as-grown thick epilayer.
23
Lifetime-limiting defects in n− 4H-SiC epilayers
P. B. Klein, B. V. Shanabrook, S. Huh et al. · Applied Physics Letters · 2006 · 218 citations