Ag films grown by remote plasma enhanced atomic layer deposition on different substrates

Akinwumi A. Amusan, Bodo Kalkofen, Hassan Gargouri, K. Wandel, C. U. Pinnow, Marco Lisker, Edmund P. Burte

Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · 2015 · 22 citations · 22 references

Concepts

Abstract

Silver (Ag) layers were deposited by remote plasma enhanced atomic layer deposition (PALD) using Ag(fod)(PEt3) (fod = 2,2-dimethyl-6,6,7,7,8,8,8-heptafluorooctane-3,5-dionato) as precursor and hydrogen plasma on silicon substrate covered with thin films of SiO2, TiN, Ti/TiN, Co, Ni, and W at different deposition temperatures from 70 to 200 °C. The deposited silver films were analyzed by x-ray photoelectron spectroscopy (XPS), atomic force microscopy (AFM), scanning electron microscopy (SEM), transmission electron microscopy (TEM) with energy dispersive x-ray spectroscopy, four point probe measurement, ellipsometric measurement, x-ray fluorescence (XRF), and x-ray diffraction (XRD). XPS revealed pure Ag with carbon and oxygen contamination close to the detection limit after 30 s argon sputtering for depositions made at 120 and 200 °C substrate temperatures. However, an oxygen contamination was detected in the Ag film deposited at 70 °C after 12 s argon sputtering. A resistivity of 5.7 × 10−6 Ω cm was obtained for approximately 97 nm Ag film on SiO2/Si substrate. The thickness was determined from the SEM cross section on the SiO2/Si substrate and also compared with XRF measurements. Polycrystalline cubic Ag reflections were identified from XRD for PALD Ag films deposited at 120 and 200 °C. Compared to W surface, where poor adhesion of the films was found, Co, Ni, TiN, Ti/TiN and SiO2 surfaces had better adhesion for silver films as revealed by SEM, TEM, and AFM images.

References

22