EngineeringElectrical EngineeringMaterials ScienceMicroelectronicsSemiconductor DevicesSemiconductor MaterialsDevice CharacterizationDevice ReliabilityHigh-frequency Semiconductor DevicesRadiation-resistant MaterialsSemiconductor ReliabilityThermal Properties Of SemiconductorsAmbient Temperature EffectsDegradationDevice DegradationGaas Microwave Integrated CircuitsHermetic PackagingHydrogen EvolutionPackage-level ReliabilityReliability Degradation
An investigation of hydrogen degradation of GaAs MMICs (MESFET, PHEMT and HBT) was conducted to determine the threshold hydrogen concentration for spacecraft application. The maximum hydrogen in the hermetic package is found to be 0.6 torr (based on 10 year mission at ambient temperature of 125/spl deg/C). Hydrogen evolution in hermetic package is also studied to determine the source of hydrogen and to minimize its level in the package. Both studies demonstrate the high reliability of hermetic A40 (Al/Si) and Kovar (Fe/Ni/Co) packages for spacecraft applications.< <ETX xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">></ETX>
2
Reliability of GaAs PHEMT under hydrogen containing atmosphere
Wenrui Hu, E.P. Parks, T. Yu et al. · 2005 · 15 citations
Reliability of state-of-the-art GaAs pseudomorphic low-noise HEMTs
Wenrui Hu, P.C. Chao, Ming-Yih Kao et al. · 2002 · 12 citations