Low Temperature Formation of Nisi2 from Evaporated Silicon

C.‐D. Lien, M‐A. Nicolet, S. S. Lau

physica status solidi (a) · 1984 · 63 citations · 14 references

Concepts

Abstract

2 MeV 4He+ backscattering spectrometry and CuKα X-ray diffraction are used to study Nisi2, formed by thermal annealing from Nisi and evaporated Si. Uniform layers of Nisi, are formed at temperatures between 350 and 425 °C. The thickness of Nisi, formed is proportional to the square root of time at a fixed temperature. This indicates that the growth of Nisi, from evaporated Si is a diffusion-controlled process. The activation energy of this reaction is about 1.65 eV, which is larger than that of regrowth of ion-implanted Nisi, and those of thermal Ni2Si and Nisi formation. The diffusion-controlled process in this case is different from the known result that on single crystal Si the formation of Nisi2 is nucleation-controlled. The dominant moving species in the present Nisi2 formation is Ni, which is identified by implanted Xe or 18O markers initially located inside the Si.

References

14