Bidimensional intercalation of Ge between SiC(0001) and a heteroepitaxial graphite top layer

L. K�ubler, Kamel Aït−Mansour, Mustapha Diani, Didier Dentel, J.L. Bischoff, M. Derivaz

Physical Review B · 2005 · 28 citations · 14 references

DOIFull text

Open access

Concepts

Abstract

High temperature annealing of $4\mathrm{H}\text{\ensuremath{-}}$ or $6\mathrm{H}\text{\ensuremath{-}}\mathrm{Si}\mathrm{C}(0001)$ crystals is well known to desorb Si from the surface and to generate a C-rich $(6\ensuremath{\surd}3\ifmmode\times\else\texttimes\fi{}6\ensuremath{\surd}3)\mathrm{R}30\ifmmode^\circ\else\textdegree\fi{}$ $(6\ensuremath{\surd}3)$ reconstruction explained as a graphite monolayer in heteroepitaxial registry with the substrate. Ge deposition at room temperature and in the monolayer range on this graphitized reconstruction results in Ge islands. Using a number of surface techniques, we follow subsequent Ge morphology evolutions as a function of isochronal post-annealing treatments at increasing temperatures. In a particular temperature window Ge reacts with the substrate by diffusion under the graphite planes and wets the Si-terminated SiC surface. In spite of this bidimensional insertion of a Ge layer, the epitaxial relationship between the SiC substrate and the graphite is maintained as shown by very clear graphite-$(1\ifmmode\times\else\texttimes\fi{}1)$ LEED or RHEED patterns. They denote extended and well-ordered graphite planes at the surface of a graphite/$\mathrm{Ge}∕\mathrm{Si}\mathrm{C}$ heterostructure. XPS analyses reveal a complete passivation of the intercalated Ge layer against oxidation by the overlying graphite sheets. Moreover, drastic spectroscopic changes on the bulk-SiC $\mathrm{Si}\phantom{\rule{0.2em}{0ex}}2p$ and $\mathrm{C}\phantom{\rule{0.2em}{0ex}}1s$ core levels are observed, depending on whether $\text{graphite}(6\ensuremath{\surd}3)∕\mathrm{Si}\mathrm{C}$ or $\text{graphite}(1\ifmmode\times\else\texttimes\fi{}1)∕\mathrm{Ge}∕\mathrm{Si}\mathrm{C}$ terminations are analyzed. In the latter case, the observed core level splitting of the bulk components is interpreted by a significant upward band bending $(\ensuremath{\sim}1.2\phantom{\rule{0.3em}{0ex}}\mathrm{eV})$ of the $n$-doped SiC, making this second interface to act as a Schottky barrier. Above $1300\phantom{\rule{0.2em}{0ex}}\ifmmode^\circ\else\textdegree\fi{}\mathrm{C}$, a delayed Ge desorption takes place that allows the graphite sheets to re-form in their initial $6\ensuremath{\surd}3$ form, i.e., without Ge and with flatter bands.

References

14