Highly Moisture-Resistive SiN<sub><i>x</i></sub>Films Prepared by Catalytic Chemical Vapor Deposition

Akira Heya, Toshikazu Niki, Yasuto Yonezawa, Toshiharu Minamikawa, Susumu Muroi, Akira Izumi, Atsushi Masuda, Hironobu Umemoto, Hideki Matsumura

Japanese Journal of Applied Physics · 2004 · 21 citations · 1 references

Concepts

Abstract

Silicon nitride (SiNx) films on Si and poly(ethylene terephthalate) (PET) substrates were prepared at approximately 150°C by catalytic chemical vapor deposition (Cat-CVD), using a SiH4/NH3 gas mixture. A water vapor transmission rate as low as 0.2 g/m2day and an O2 gas transmission rate of 0.6 cm3/m2day were achieved for a stoichiometric Si3N4 film of 77 nm thickness. Although these transmission rates depended on N/Si ratio, no optical absorption was observed under preferable deposition conditions.

References

1