Japanese Journal of Applied Physics · 2000 · 17 citations · 4 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMicroelectronicsThin FilmsElectrode MaterialsFerroelectric CeramicsFerroelectric MaterialsPerovskite MaterialsSemiconductor Device MaterialsThin Film Electrical PropertiesCrystallizationCrystallization Induced By AnnealingDamascene ProcessFabricationFerroelectric CapacitorsLeakage CurrentMechanical PolishingPerovskite Crystal Structure
Submicron ferroelectric capacitors were fabricated by a damascene process using chemical mechanical polishing (CMP). The fabricated capacitors consisted of SrBi 2 Ta 2 O 9 (SBT) film with top and bottom electrodes of IrO 2 films. The capacitor size was 0.8 µm in diameter, that is, 0.5 µm 2 in area. Damage by the fabrication process was not observed in electrical measurements, such as the dependence of remanent polarization on electric field and leakage current properties. The remanent polarization (2Pr) of 5 µC/cm 2 at the saturation voltage of 2 V is half that of a large capacitor because the SBT films were composed of single-crystal grains in the bismuth-layered perovskite structure and micro-crystals in many phases including pyrochlore. The crystallinity of the SBT films may be associated with the redistribution of Bi between the SBT thin films and the IrO 2 electrodes during the crystallization annealing of SBT.
4
Ichiro Koiwa, Yukihisa Okada, Juro Mita et al. · Japanese Journal of Applied Physics · 1997 · 36 citations
Natural Sciences, Materials Engineering, Materials Science +15