Natural SciencesMaterials EngineeringMaterials ScienceMaterials CharacterizationMaterials ChemistryThin FilmsAmorphous MaterialsAmorphous SolidsCalorimetrySilicon MaterialsThin-film MaterialsAmorphizationExothermic Reaction KineticsExothermic TransitionsGibbs Free EnergyGibbs Free Energy AnalysisSiliconSilicon ChemistryX-ray Diffraction Analysis
The mechanisms of the formation of titanium silicide from the reaction of a single thin film of Ti on the silicon substrate with different degrees of substrate amorphization were studied using differential scanning calorimetry. With increased amorphization, an exothermic reaction prior to C49-TiSi2 formation was observed. X-ray diffraction discovered an unidentified phase together with Ti5Si3 and Ti5Si4 that disappeared with subsequent formation of C49-TiSi2 at temperatures above 650 °C. The difference in Gibbs free energy was considered in explaining the formation of Ti5Si3 and Ti5Si4. Based on the Scherrer equation, the resultant C49-TiSi2 grains with higher degrees of silicon substrate amorphization were smaller than those without silicon substrate amorphization.
13
Thermochemical data of pure substances
Choice Reviews Online · 1993 · 4.5K citations
Zhenqiang Ma, L. H. Allen · Physical review. B, Condensed matter · 1994 · 143 citations
Natural Sciences, Materials Engineering, Materials Science +16
High Temperature Process Limitation on TiSi2
C. Y. Ting, F. M. d’Heurle, Subramanian S. Iyer et al. · Journal of The Electrochemical Society · 1986 · 117 citations