Japanese Journal of Applied Physics · 2000 · 19 citations · 9 references
EngineeringMaterials EngineeringMaterials ScienceElectrochemistryMicrofabricationSemiconductor DevicesEtching ProcessesIntegrated Circuit FabricationMicrofabrication MaterialsMicrofabrication ProcessesSubstrate PreparationDevice FabricationElectropolishingSilicon MicrostructuresSilicon Wafer ProcessingSilicon WafersWafer Materials
Through-holes were formed by selective partial electropolishing in a 2.5 wt% HF electrolytic solution, using an N-type, (100)-oriented Si wafer as an anode, and a Pt plate as a cathode. The obtained holes were square through-holes of 5–35 µm side length, with an aspect ratio of 109. It was possible to form such through-holes with a density of 3,500 holes/mm 2 in specified areas. It was also confirmed that the pit of the square-based inverted pyramid structure could form deep capillaries. This suggests the possibility of forming microstructures such as pillars and tubes.
9
Porous silicon formation mechanisms
R. L. Smith, Scott D. Collins · Journal of Applied Physics · 1992 · 1.2K citations
Electrolytic Shaping of Germanium and Silicon
A. Uhlir · Bell System Technical Journal · 1956 · 1.1K citations