Applied Physics Letters · 1987 · 28 citations · 9 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsDopingImplant MaterialsImplant TechnologyIon ImplantationSemiconductor Device MaterialsSilicon MaterialsActivationCarrier ConcentrationCarrier MobilityCharge Carrier MobilityRapid Thermal AnnealingSilicon AnnealingSilicon DopingThermal Annealing
Rapid thermal annealing has been used to electrically activate Si-implanted InP:Fe. A two-step annealing cycle in which the short (5 s) high-temperature step is followed by a relatively long (25–60 s) 100 °C lower temperature step gave higher activation and carrier mobility than the corresponding short high-temperature or long low-temperature single step annealing cycle. A good surface morphology was achieved by using InP proximity anneal if the maximum annealing temperature is limited to 900 °C for not more than 5 s. The maximum mobilities and activations obtained for 200 keV/5×1013 cm−2 and 150 keV/1×1013 cm−2 Si+ implants were 1740 and 2260 cm2/V s and 88 and 98%, respectively. The position of the peak carrier concentration in the depth profile closely matched that of the Lindhard–Scharff–Schiott prediction.
9