Applied Physics Letters · 1993 · 63 citations · 10 references
EngineeringMaterials EngineeringMaterials ScienceMaterials ChemistrySemiconductor MaterialsSpectroscopyDefects In Electronic MaterialsOptical Properties Of SemiconductorsPorosity CharacterizationSemiconductor DefectsSemiconductor Device MaterialsSilicon MaterialsDefect DensityDefect StatesInfrared EmissionPorous SiliconSiliconSilicon AnnealingSilicon DefectsSilicon Dioxide
The defect properties of as-etched and annealed porous silicon are studied by electron paramagnetic resonance (EPR) and optically detected magnetic resonance (ODMR). The paramagnetic defect observed is closely related to the Pb0 center at the Si/SiO2 interface. In EPR a minimum defect density of 1016 cm−3 is observed for the as-etched silicon, which reaches a maximum of 8×1018 cm−3 for samples annealed at about 400 °C. In the ODMR experiments, the same dangling bond center is observed on the 1.5 eV luminescence band enhancing the luminescence—but with increased sensitivity and as a decrease of the emission intensity in the infrared emission band at 1 eV of porous silicon.
10
Rapid-thermal-oxidized porous Si−The superior photoluminescent Si
V. Petrova-Koch, T. Muschik, A. Kux et al. · Applied Physics Letters · 1992 · 466 citations
Natural Sciences, Materials Engineering, Materials Science +17
Luminescence degradation in porous silicon
M. A. Tischler, R. T. Collins, J. H. Stathis et al. · Applied Physics Letters · 1992 · 465 citations
Natural Sciences, Materials Engineering, Materials Science +17