The Influence of Phosphorus Concentration of Electroless Plated Ni-P Film on Interfacial Structures in the Joints between Sn-Ag Solder and Ni-P Alloy Film

Takao Komiyama, Yasunori Chonan, Jin Onuki, Toshihiko Ohta

MATERIALS TRANSACTIONS · 2002 · 12 citations · 4 references

DOIFull text

Open access

Concepts

Abstract

The interface structure between Sn–3Ag solder and electroless plated Ni film and the structure near that interface were examined. Plated electroless Ni films contained 3.7 mass% phosphorus or 8.5 mass% phosphorus. A P-enriched layer is formed at the joining interface between plated electroless Ni film and Sn–3Ag solder, in each sample with 3.7 mass%P and 8.5 mass%P. P-enriched layers of both P concentration samples contained double the P concentration than the original plated Ni films. Also, the P-enriched layer of the Ni–8.5 mass%P sample was much thicker than that of the Ni–3.7 mass%P sample. Both P-enriched layers have been composed of Ni–Sn–P layer and P enriched Ni–P layer. Kirkendall voids were formed between the 1st Ni–Sn–P layer and 2nd Ni–P layer. The number of voids observed in Ni–8.5 mass%P sample was much greater than those in the Ni–3.7 mass%P sample. Intermetallic compounds, mixtures of Ni3Sn2 and Ni3Sn4, were formed by the interfacial reaction. In the case of the Ni–3.7 mass%P sample, Ni–Sn intermetallic compounds continuously crystallized on the P-enriched layer, while in the case of the Ni–8.5 mass%P sample, Ni–Sn intermetallic compound crystallized dispersively in the solder.

References

4