Physical review. B, Condensed matter · 1993 · 25 citations · 23 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsThin FilmsDefect CharacterizationDefectsDefects In Electronic MaterialsSemiconductor DefectsSemiconductor PhysicsSemiconductor Thin FilmsElectronic DefectsImpurity DefectsMolecular Beam EpitaxyNative Oxide RemovalPoint DefectsSemiconductor CharacterizationSensitivitySilicon Defects
Positron annihilation in Si is a quantitaive, depth-sensitive technique for the detection of vacancylike defects or voids. A sensitivity of 5\ifmmode\times\else\texttimes\fi{}${10}^{15}$ ${\mathrm{cm}}^{\mathrm{\ensuremath{-}}3}$ for voidlike defects is easily achieved. The technique has been applied to a study of point-defect distributions in thin films of Si grown by molecular-beam epitaxy. A special procedure was developed to remove the influence of the native oxide on the positron measurement. 200-nm-thick films grown at temperatures between 475 and 560 \ifmmode^\circ\else\textdegree\fi{}C show no defects below the sensitivity limit and are indistinguishable from the bulk substrate. So are films grown at 220 \ifmmode^\circ\else\textdegree\fi{}C, provided a 2-min high-temperature anneal to a peak temperature of \ensuremath{\ge}500 \ifmmode^\circ\else\textdegree\fi{}C is executed every \ensuremath{\simeq}30 nm during growth. If ${\mathit{T}}_{\mathrm{RTA}}$=450 \ifmmode^\circ\else\textdegree\fi{}C, part of the film contains vacancylike defects to a concentration of \ensuremath{\simeq}${10}^{18}$ ${\mathrm{cm}}^{\mathrm{\ensuremath{-}}3}$. These results correlate well with current-voltage characteristics of p-n junctions grown with different rapid thermal anneal (RTA) temperatures. Ion scattering, with a defect sensitivity of \ensuremath{\approxeq}1%, shows no difference between films grown with different ${\mathit{T}}_{\mathrm{RTA}}$. Recrystallization of amorphous films, deposited at room temperature and annealed in situ at 550 \ifmmode^\circ\else\textdegree\fi{}C, always leaves a significant defect concentration of \ensuremath{\simeq}2\ifmmode\times\else\texttimes\fi{}${10}^{18}$ ${\mathrm{cm}}^{\mathrm{\ensuremath{-}}3}$; those defects are reduced but still present even after a 2-h 800 \ifmmode^\circ\else\textdegree\fi{}C furnace anneal.
23
The physics of semiconductor devices
H. L. Grubin · IEEE Journal of Quantum Electronics · 1979 · 2.8K citations
Ideal hydrogen termination of the Si (111) surface
G. S. Higashi, Yves J. Chabal, Gary W. Trucks et al. · Applied Physics Letters · 1990 · 1.4K citations