IEEE Transactions on Electron Devices · 2018 · 30 citations · 37 references
EngineeringElectrical EngineeringMaterials ScienceElectronic MaterialsMicroelectronicsSemiconductor DevicesDevice ScalingIntegrated Circuit DesignMemory DevicesDoped SemiconductorsDynamic Random-access MemoryMemory Circuit DesignNon-volatile Memory DesignRandom-access MemoryScalabilityTransistor ScalingTransistor Sizing
This paper reports on the usefulness of shell-doped (SD) junctionless (JL) transistor architecture for operation as capacitorless dynamic random-access memory (1T-DRAM). SD topology overcomes the problem associated with shallower potential depth in heavily doped devices, thereby enhancing the retention time (RT) along with improved scalability. The use of a thinner shell for achieving high RT is beneficial as it reduces generation and recombination of holes. The results show that an undoped core region with shell thickness (T <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Shell</sub> ) of 2 nm yields maximum retention. An SD (Nd) of 10 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">18</sup> cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">-3</sup> attains RT of ~5.5 s and ~630 ms at 27 °C and 85 °C, respectively, whereas higher N <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">d</sub> (1019 cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">-3</sup> ) shows RT of ~13 ms at 85 °C for L <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">g</sub> = 200 nm. SD JL transistor shows less degradation in RT with temperature. A 10 nm SD JL device with RT of ~11 ms at 85 °C demonstrates applicability as 1T-DRAM at shorter gate lengths.
37