International Journal of Electronics · 1998 · 17 citations · 27 references
Natural SciencesMaterials SciencePhysicsElectronic MaterialsMaterials PhysicsThin FilmsAmorphous MaterialsConductive MaterialsElectrical CharacterizationElectrical ConductivitySemiconductor PhysicsThin Film Electrical PropertiesAmorphous SeleniumAnnealing Temperature EffectsConductionDangling Bond DefectsElectronic ConductionTemperature DependenceTemperature Dependence Of Electrical PropertiesTemperature-dependent Conductivity
Abstract The linear DC dark- and photo-current-voltage characteristics observed for as deposited (Ts=25°C) and annealed (Ta=70°C) thermally-evaporated selenium s a films in the temperature range 150-300K were used to deduce the respective temperature dependencies of the dark-conductivity σdark and photo-conductivity σph of these samples. Both XRD and SEM studies confirmed the amorphous state ph of the as-deposited films and the hexagonal-like polycrystalline structure of the annealed films. The ln σ versus 1/T plots of the highly resistive amorphous selenium (a-Se) samples revealed only one thermally-activated process in the region 250-300K for both σdark and σph with an activation energy Eσ= 0.73eV, dark ph sigma and 0.49eV, respectively. This has been interpreted considering the conduction models based on the existence of the inherent charged defect centres (dangling bonds D−, D+) in the band tails. The conductivity of the annealed specimens was at least three orders of magnitude larger than that of the as-deposited ones and the temperature-dependence of their σdark and σph exhibited two different dark ph conduction mechanisms; one being operative in the high-temperature region (230-300K) and the other being dominant at low temperatures (220-150K). As these annealed samples were polycrystalline, the former activated process has been analysed on the basis of grain-boundary-limited conduction with Eσ= 0.17eV (σdark) and 0.15eV (σph). The low-temperature conductivity of these sample has dark ph been described in terms of variable range hopping conduction, of Mott's type, which appears to be applicable in polycrystalline solids at relatively low temperatures. The observed reduction in the grain-boundary potential barriers and in the degree of disorder on illuminating the annealed selenium films has been understood by the phenomenon of neutralization of the native dangling bond states present at the interface of the grain boundaries of these samples by the photo-generated charge carriers.
27
Electronic Transport in Amorphous Silicon Films
P. G. Le Comber, W. E. Spear · Physical Review Letters · 1970 · 453 citations