Bipolar transistor fabrication in low-temperature (745°C) ultra-low-pressure chemical-vapor-deposited epitaxial silicon

Wolfgang Bürger, J.H. Comfort, L. M. Garverick, Tri‐Rung Yew, R. Reif

IEEE Electron Device Letters · 1987 · 19 citations · 0 references

Concepts

Abstract

In this letter we report for the first time the successful fabrication of bipolar transistors in low-temperature (T <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">dep</inf> = 745°C) epitaxial silicon deposited by a chemical-vapor-deposition (CVD) technology. The epitaxial layers were deposited by an ultra-low-pressure CVD (U-LPCVD) technique utilizing an optimized in-situ predeposition argon sputter clean. The critical parameter during the sputter clean has been identified as the substrate bias. Bias voltages of -200 or -300 V create dislocations that form emitter-collector shunts during the bipolar transistor fabrication process; a bias voltage of -100 V, however, permits the deposition of essentially defect-free (<10 dislocations cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">-2</sup> by defect etching) epitaxial films suitable for bipolar transistor fabrication.