Journal of Vacuum Science and Technology · 1979 · 47 citations · 0 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsThin FilmsDopingEpitaxial GrowthSemiconductor InterfacesSemiconductor PhysicsSemiconductor Thin FilmsSilicon MaterialsCarrier ConfinementEpitaxial Film GrowthFilm ThicknessHall EffectMolecular Beam EpitaxyMolecular Beam ExperimentsSemiconductor Doping ProfilesSilicon Doping
Silicon epitaxial films are deposited on 51-mmφ Si substrates by the molecular beam technique. Silicon and the dopant antimony are evaporated from separate sources. Typical process conditions before and during the growth are as follows: substrate heat cleaning at 1173 K for five minutes, substrate temperature 1023 K, growth rate 1 μm/h, film thickness between 0.1 and 3 μm. This procedure is found to be sufficient for obtaining dislocation-free films. The total Sb concentration in the MBE films is measured by neutron activation analysis, the electrically effective concentration with Hall or C–V measurement. Carrier concentrations between 3×1014 and 2×1019 cm−3, and Hall mobilities between 100 and 1400 cm2/V s are obtained. Profiles of the total Sb concentration and of the carrier concentraton with its extremely abrupt substrate-to-epilayer interface elucidate the advantage of the low-temperature MBE technique.